Effects of Varying Humiditiy in Polymers by Nanoindentation: Investigation of the Effects of Varying Humidity in Additive Manufactured by Depth Sensing Indentation - Kazim Altaf - Books - LAP LAMBERT Academic Publishing - 9783845430508 - September 5, 2011
In case cover and title do not match, the title is correct

Effects of Varying Humiditiy in Polymers by Nanoindentation: Investigation of the Effects of Varying Humidity in Additive Manufactured by Depth Sensing Indentation

Price
€ 62.99

Ordered from remote warehouse

Expected delivery Nov 25 - Dec 3
Christmas presents can be returned until 31 January
Get notified about new Kazim Altaf releases
Add to your iMusic wish list

Not rated yet

Stereolithography is one of the main additive manufacturing methods and is considered highly accurate and consistent, however, polymers used in the process are highly hygroscopic and moisture absorption decreases mechanical strength. Investigation of the effects of moisture on polymers can be carried out using a number of experimental techniques; however, the benefits of the depth sensing indentation or nanoindentation method over bulk tests include its ability to characterise various mechanical properties in a single test from only a small volume of material and the investigation of spatial variation in mechanical properties near the surface. The experimental and FE modelling methodologies proposed in this work provide a validated and systematic approach for characterising and predicting moisture degradation in additive manufactured components under varying environmental conditions on submicron scale. Work also compares the analysis of indentation data using the Oliver and Pharr method with those derived from viscoelastic-plastic material models. It is argued to use time-dependent material models when characterising indentation response of materials such as polymers and bio-material.

Media Books     Paperback Book   (Book with soft cover and glued back)
Released September 5, 2011
ISBN13 9783845430508
Publishers LAP LAMBERT Academic Publishing
Pages 284
Dimensions 150 × 16 × 226 mm   ·   441 g
Language German  

More by Kazim Altaf